Weighted silk
Weighted silk has been loaded with metallic salts, usually tin or iron, to replace weight lost in degumming; the salts make it split with age.
Weighted silk has been treated with metallic salts so that it weighs, and sells for, more. The practice peaked in the late nineteenth century, and the salts are a main reason why silks of that period split and shatter.
Why was silk weighted?
Boiling off the natural gum, sericin, leaves silk softer but lighter. The Canadian Conservation Institute explains that makers restored that lost weight, and added body, with metallic salts such as tin chloride. They rarely stopped at replacement. Matthews reported in 1913 that black-dyed silks were especially liable to heavy loading, sometimes 400 percent or more, with Prussian blue and iron tannate for blacks and tin phosphate for colors. US labeling rules later drew a line: by 1970 the National Bureau of Standards could state that "pure silk" must contain no metallic weighting, and that a weighted silk's label must give the percentage.
How do you recognize it, and why does it matter?
In a burn test, CCI notes that only weighted silk leaves a very fine ash in the shape of the yarn or fabric structure; Matthews described the same effect, a silk that will not flame but smolders to a coherent ash. The hand is not a reliable guide: a 1989 study of 54 historic silks found that not all weighted silks were crisp or stiff. That study also found that tin above 3 percent appeared particularly damaging, leaving yarns with almost no strength, and Matthews had already measured black silk weighted 140 percent at less than one sixth the strength of raw silk. The end state is the brittle splitting conservators call shattered silk.
Sources
- Natural Fibres (CCI Notes 13/11). Canadian Conservation Institute
- The Identification of Natural Fibres (CCI Notes 13/18). Canadian Conservation Institute
- The Textile Fibres: Their Physical, Microscopical and Chemical Properties. J. Merritt Matthews, The Textile Fibres, 3rd ed. (John Wiley & Sons, 1913)
- Degradation in Weighted and Unweighted Historic Silks (Miller and Reagan). Journal of the American Institute for Conservation 28(2), 1989
- Fibers and Fabrics (Blandford and Gurel). National Bureau of Standards, Consumer Information Series 1, 1970